This is wrong repairing bubbles once cured is very difficult or nearly impossible without needing to re coat.
Air bubble roller popper for floor coatings.
Eliminate any source of direct air blowing onto the surface.
Bubbles sometimes form within the coating or on the backside of the coating film.
These pinholes are caused by air bubbles formed in the epoxy coating during the application process.
Avoid aggressive shot blasting.
Various nap roller covers have air within them.
Rapid stirring for a prolonged period can introduce air bubbles into the paint that might persist in the dried paint coat.
Fixes during prime coat installation.
Apply paint gradually if using a roller.
For example moisture cured urethane mcu coatings that dry and cure by reaction with atmospheric moisture and other coating types i e aliphatic polyurethanes that are formulated with moisture sensitive components can also bubble.
Using a roller to pick out the bubbles from the floor.
Aides in flow out and leveling.
Effectively remove air bubbles from an epoxy coating using acetone spray technique.
If air bubbles are present in coating allow to sit briefly before pouring on the floor.
Follow label and data page directions for the appropriate applicator.
Epoxy floor coating problem solving guide page 10 prevention.
Allow the coating to dry thoroughly then sand the coating smooth and repaint.
If you see bubbles forming in.
Spike rollers can be used if bubbles appear but may not completely remove them.
Air moving in and out of the concrete slab with changes in temperature and barometric pressure.
Little pinholes in the floor.
After applying coatings with a squeegee you should never take a dry roller cover and roll out the floor.
Use this technique for removing air bubbl.
Always follow recommended nap and type of cover.
Concrete that has not been cured properly and is soft punky.
If there is a very noticeable amount of air bubbles during application try slowing down application speed.
This can often prevent the outgassing bubble from forming and allow the primer to fill in the pinhole that would otherwise be created.
We recommend saturating your 9 or 18 roller cover in the product and then rolling it and make it.
Follow directions for mixing and using primer.
Use a primer system on all porous concrete.
If outgassing bubbles are seen during the primer application a metal porcupine roller can be used to pop the surface tension as bubbles start to develop.
Some people mistakenly assume that they appear later once the floor has cured.
If bubbles are seen while applying the primer a metal porcupine roller can be used to pop the surface tension as bubbles start to develop.
Woven shed resistant rollers are recommended.